Technical Data Sheet #34

ZINC CORROSION

Corrosion behavior of galvanized steel

Corrosion protection for steel is often thought of as applying a coat of paint or another similar coating. A paint system covers the steel surface to prevent rust.

Effective protection requires not only a suitable paint system but also sufficient film thickness and professional application. The raw materials and additives in the paint ensure good workability and give the cured paint film the necessary resistance to environmental influences. In principle, a properly cured paint film does not react with the steel substrate.
A completely different form of corrosion protection is the application of a metallic coating. This collective term encompasses all kinds of metals that can provide protection and/or aesthetic enhancement. This fact sheet specifically addresses metallic coatings made of zinc. Unlike a paint coating, a zinc coating is reactive.
Whereas a paint coating hardly reacts with the environment after curing and only loses its protective effect (and develops brown iron rust) due to aging, wear, or damage, zinc actually reacts with substances in the ambient air. As a result, the thickness of the zinc coating gradually decreases over time. This natural process is called zinc corrosion. Under normal atmospheric conditions, however, this is a beneficial phenomenon. During the corrosion process, a dense and well-adhering zinc patina forms, which shields the underlying zinc layer and significantly reduces the rate of further corrosion. As a result, zinc corrodes much more slowly than steel, and the steel remains protected for a long time.

SEE TECHNICAL DATA SHEET 36: FORMATION OF THE ZINC COATING

SUMMARY

Both paint coatings and metallic coatings protect steel from corrosion. However, the way in which this protection is achieved differs significantly. A galvanized coating employs a different protective mechanism than a paint system. This also requires a different approach to corrosion protection and the system’s service life.

EFFECT OF ATMOSPHERIC CONDITIONS

The chemical composition of the zinc patina layer also determines the corrosion rate of zinc. That composition is determined by substances present in the atmosphere. Therefore, it is essential to correctly assess the environment in which the galvanized steel will be used. Only then can a reliable estimate of the maintenance-free service life be made.
The end of the maintenance-free service life does not mean that the steel has suddenly corroded completely. Corrosion is a gradual process. In the standards, the maintenance-free service life is defined as the point at which approximately 5% of the steel surface shows signs of rust.
From that point on, various measures can be taken. Localized corrosion can be repaired, the object can be hot-dip galvanized again, or a paint system can be applied to further extend its service life.
The corrosion rates of steel and zinc under various atmospheric conditions are specified in international standards, including ISO 9223, ISO 12944-2, and ISO 14713-1. These standards classify environments into corrosion categories, ranging from C1 (very low) to CX (very high).

When using hot-dip galvanized steel, it is advisable to assess the local environment. Be sure to also examine existing hot-dip galvanized structures, such as fences, light poles, bike racks, or other steel objects that have been exposed to the same environment for many years. The condition of these objects often provides a good indication of the expected maintenance-free service life.
The situation described above relates to atmospheric corrosion. In this process, the zinc layer reacts with substances in the ambient air, causing the zinc to corrode gradually and form a protective patina layer.
Another form of corrosion occurs when zinc comes into contact with acidic or basic substances. Zinc is, in fact, an amphoteric metal, which means it is sensitive to the pH (acidity) of a liquid. If it is soluble at both low and high pH levels, it is referred to as an amphoteric metal. Acidic conditions can arise, for example, from decaying organic material such as manure, leaves, blossoms, or fruit. Strongly basic conditions occur, among other things, in caustic soda and concrete. As long as concrete has not yet hardened and therefore still contains a wet fraction, the pH is high.
When galvanized steel is not exposed to the atmosphere but is used, for example, in soil or water, predicting its maintenance-free service life is considerably more complex. In such cases, numerous factors come into play, and a separate assessment is necessary.

SEE TECHNICAL DATA SHEET 24: GALVANIZED STEEL IN THE GROUND

zinc patina

In addition to atmospheric corrosion, electrochemical corrosion can also occur. This phenomenon occurs when two different metals are in electrical contact with each other and a conductive liquid, such as (contaminated) rainwater or surface water, is present. This creates a Voltaic cell (in 1800, Alessandro Volta invented the Voltaic pile, an early electric battery that provided a constant electric current).
An electric circuit is formed in which ions are released by a base metal when a more noble (or less base) metal serves as the cathode. In this process, zinc acts as the anode and releases ions. Such a situation can occur, for example, when galvanized steel comes into contact with copper in the presence of (contaminated) rainwater or surface water.

PRACTICAL EXAMPLES OF ENVIRONMENTS THAT REQUIRE EXTRA ATTENTION

The galvanized coating is susceptible to atmospheres containing chlorides (salts). This results in a thinner zinc patina layer, which accelerates the rate of zinc corrosion. When people think of chloride exposure, they often think of seawater and swimming pool water, but chlorides also come from deicing salts used to prevent icing on roads, bridges, and, for example, the walkways of apartment buildings. Unlike sea salt, road de-icing salt is much more aggressive. For this reason, galvanized steel in coastal areas of the Netherlands and Belgium generally poses no problem whatsoever with regard to salt exposure. Galvanized products used directly on the beach may also be exposed to wear caused by wind-blown sand. The abrasive action of sand particles carried by the sea breeze prevents the formation of the zinc patina layer and can cause the zinc coating to gradually wear away.
In industrial areas with potentially severe environmental stress, such as the ports of Rotterdam and Ghent, other chemical substances may also play a role in determining service life. These include sulfur dioxide, soot, dirt, chemicals, and curing gas (ethylene gas).

HOW TO PREVENT THE EFFECTS OF HARMFUL CHEMICALS AND GASES

When zinc is exposed to substances in the atmosphere, soil, or ground that are harmful to the zinc layer, it may be advisable to apply a suitable organic coating over the galvanized layer.
Liquid paint systems and powder coatings form a protective barrier, thereby better protecting the zinc coating against corrosive influences. In addition, it may be advisable to first expose freshly galvanized materials to clean outdoor air for a period of time, allowing a suitable zinc patina to form before the structure is installed at its final location. A few weeks of storage in a rural environment, free from disruptive chemicals, can work wonders in this regard. It is also possible for a fresh zinc coating to be directly exposed to a humid environment, for example during a rainy period or due to condensation. This can cause wet storage stains. These are often mistakenly referred to as “white rust.”

Zinc corrosion in the form of "white rust"

SUMMARY

Zinc is a metal that gives steel structures an exceptionally long, maintenance-free service life. Hot-dip galvanizing is a unique and proven method for providing steel with long-lasting protection against corrosion. At the same time, zinc is a reactive metal with specific properties. That is why it is important to carefully assess, for each application, the conditions under which the galvanized steel will be used.
This technical information sheet provides guidance for that assessment. Do you have questions about your specific application? Please feel free to contact your galvanizing plant or the Zinkinfo Benelux help desk.

EN ISO 14713 part 1
Zinc coatings – Guidelines and recommendations for the protection of iron and steel in structures against corrosion – Part 1: General design principles and corrosion resistance.

EN ISO 14713 part 2
Zinc coatings – Guidelines and recommendations for the protection of iron and steel in structures against corrosion – Part 2: Hot dip galvanizing

ISO 9223
: Corrosion of metals and alloys—Atmospheric corrosion severity—Classification, determination, and estimation

ISO 12944-2
Paints and varnishes — Protection of steel structures against corrosion by protective paint systems — Part 2: Classification of environments

TECHNICAL DATA SHEET 1
Stains Caused by Storage in Damp Conditions

TECHNICAL DATA SHEET 4
Contact Corrosion and How to Prevent It

TECHNICAL DATA SHEET 10
Corrosion Resistance of Galvanized Steel

TECHNICAL DATA SHEET 24
Galvanized steel in the ground

TECHNICAL DATA SHEET 25
Zinc Patina: Formation and Protection

TECHNICAL DATA SHEET 26
Ensuring the Adhesion of the Zinc Coating

TECHNICAL DATA SHEET 36
Formation of the zinc coating